Hebei Key Laboratory of Modern Metallurgical Technique, College of Metallurgy and Energy, North China University of Science and Technology, Tangshan 063009, Hebei, China
In order to achieve high gasification dephosphorization of high-phosphorus iron ore after sintering,promote the development and utilization of high-phosphorus iron ore,the influence of material com-position on the gasification dephosphorization rate had been investigated via microwave heating. When u-sing bituminous coal,5% C/O,0.75% SiO2 addition,1.5% CaCl2 addition and 1.4 of alkalinity, high-phosphorus iron ore fines could be achieved 20.36% of gasification dephosphorization in the microwave field. X-ray diffraction(XRD) results on the calcined product found out that excessive addition of CaCl2 would produce Ca5(PO4)3Cl, and not favorable for gasification dephosphorization.