[1] | Zheng Kui, Wang Wei, Gan Xian, Xie Hong’en, Fu Weiguo, Dong Xiaosen. Research on theoretical combustion temperature control of V-Ti magnetite blast furnace smelting[J]. IRON STEEL VANADIUM TITANIUM, 2024, 45(5): 130-138. doi: 10.7513/j.issn.1004-7638.2024.05.017 |
[2] | Dong Yafeng, Guo Peimin, Liu Keming, Zhai Dan. Industrial Test of Titanium Powder and Pulverized Coal Co-injection[J]. IRON STEEL VANADIUM TITANIUM, 2020, 41(6): 99-106. doi: 10.7513/j.issn.1004-7638.2020.06.018 |
[3] | Yan Chaojie, Chen Shujun, Zhao Xiaojie, Li Fumin, Lü Qing, Qie Yana. Experimental Study on Reduction of Vanadium Oxides in Blast Furnace Hearth[J]. IRON STEEL VANADIUM TITANIUM, 2017, 38(1): 22-26,37. doi: 10.7513/j.issn.1004-7638.2017.01.004 |
[4] | Wu Hao, Zou Chong, Zhao Junxue, Li Xiaoming. Properties of BOF dust and its effect on combustion of pulverized coal[J]. IRON STEEL VANADIUM TITANIUM, 2017, 38(5): 84-89. doi: 10.7513/j.issn.1004-7638.2017.05.016 |
[5] | Dong Xiaoxu, Zhang Shuhui, Lan Chenchen, Lü Qing. Study on Dealkalization Capacity of BF Slag with Low Titanium Content[J]. IRON STEEL VANADIUM TITANIUM, 2016, 37(6): 99-102. doi: 10.7513/j.issn.1004-7638.2016.06.018 |
[6] | Li Yanjiang, Lü Qing, Lu Jianguang, Liu Xiaojie, Huang Honghu, Wang Yan. Injection of Gravity Precipitator Dust into Blast Furnace[J]. IRON STEEL VANADIUM TITANIUM, 2015, 36(6): 57-62. doi: 10.7513/j.issn.1004-7638.2015.06.011 |
[7] | Deng Yongchun, Jia Suqi, Wu Shengli, Jiang Yinju. Removal of the Harmful Elements and Iron Recovery from the Blast Furnace Gas Ash by Chloridizing Roasting[J]. IRON STEEL VANADIUM TITANIUM, 2015, 36(6): 51-56. doi: 10.7513/j.issn.1004-7638.2015.06.010 |
[8] | Feng Xuewu, Jin Yan, Li Yang, Cheng Changgui, Chang Zhengsheng, Jin Yelei. Analysis of BF Flow Field before and after Slag Formation[J]. IRON STEEL VANADIUM TITANIUM, 2015, 36(5): 122-128. doi: 10.7513/j.issn.1004-7638.2015.05.023 |
[9] | LIU Zengxun, Lü Qing. Heat Transfer Analysis for Slag Skull Thickness of Blast Furnace[J]. IRON STEEL VANADIUM TITANIUM, 2008, 29(3): 51-54. |
[10] | Du Sihong. Investigation on Improving Combustion Properties of Blast Furnace Pulverized Coal Injection[J]. IRON STEEL VANADIUM TITANIUM, 2007, 28(2): 43-47. |
[11] | GUO Shu-yi, CHEN Ju-hua. STUDY ON DYNAMICAL MECHANISM IN BLAST FURNACE RACEWAY[J]. IRON STEEL VANADIUM TITANIUM, 2004, 25(3): 1-4,9. |
[12] | LIU Shu-fang. TECHNICAL MODERNIZATION OF NO.1 BLAST FURNACE RELINING AT PZH STEEL[J]. IRON STEEL VANADIUM TITANIUM, 2002, 23(4): 59-64. |
[13] | LI Zhen-cai, ZHANG Wen-xin, RAO Jia-ting, FAN Yun-dong, ZHONG Yu-ming, WANG Hua. AN INDUSTRIAL-SCALE EXPERIMENT UPON INJECTION OF MIXING PULVERIZED COALS INTO BLAST FURNACE AT PZH STEEL[J]. IRON STEEL VANADIUM TITANIUM, 2000, 21(4): 5-8. |
[14] | DIAO Ri-sheng, LIU Shu-fang, YANG Zhi-yuan. OPERATION PRACTICE OF NUT COKE RECOVERY AND MIXED CHARGING FOR PZH STEEL BLAST FURNACE[J]. IRON STEEL VANADIUM TITANIUM, 2000, 21(1): 45-49. |
[15] | Zhong Yong, Zhao Daiqiong, Jiang Sheng. MEASURES FOR REDUCTION OF COKE RATE OF BF IRONMAKING AT PANGANG[J]. IRON STEEL VANADIUM TITANIUM, 1999, 20(2): 57-62. |
[16] | Liu Shufang, Li Pingwei, Xie Junyong. LONG CAMPAIGN LIFE PRACTICE OF 4# BLAST FURNACE AT PANGANG[J]. IRON STEEL VANADIUM TITANIUM, 1999, 20(1): 6-10,15. |
[17] | Qi Shuangyang, Li Hongfang, Jiang Sheng, Shi Shixiong, Rao Jiating, Diao Risheng, Zhang Shankun, Guan Yong. STUDY OF COMBUSTION SCHEDULE FOR IMPROVED INTERNAL COMBUSTION HOT STOVE[J]. IRON STEEL VANADIUM TITANIUM, 1999, 20(3): 37-42,64. |
[18] | ZHONG Yong. A MATHEMATICAL MODEL FOR ESTIMATING GAS FLOW DISTRIBUTION IN THE BLAST FURNACE THROAT[J]. IRON STEEL VANADIUM TITANIUM, 1998, 19(3): 59-64. |
[19] | Qing Shangsheng, Chen Jingju, Luo Chuanyue, Liu Shufang. STUDY AND APPLICATIONS OF ABRASION RESISTANT LINING PLATE──USED IN THE FEEDING, CONVEYING AND MIXING SYSTEM FOR BF[J]. IRON STEEL VANADIUM TITANIUM, 1995, 16(2): 9-15. |
[20] | Li Zbencai. TEST ON MAINTAINING TEMPERATURE OF THE SKIMMER OF BF AT PANZHIHUA IRON AND STEEL CO.[J]. IRON STEEL VANADIUM TITANIUM, 1994, 15(4): 61-66. |