Analysis on Metallographic Structure and Surface Defect of Heat-resistant Austenitic Stainless Steel 309S
-
摘要: 通过冶炼—轧制—退火酸洗工艺生产309S奥氏体耐热不锈钢卷板,研究其连铸板坯、轧制态以及退火态金相组织,退火态力学性能和表面缺陷。结果表明:309S奥氏体耐热不锈钢在三种状态下的组织均为奥氏体相和残留的高温铁素体相,这种高温铁素体难以通过热处理消除;轧制态和退火态金相组织中,厚度方向近表面铁素体含量少,心部铁素体含量高;高温铁素体的存在不影响产品的力学性能;通过连铸板坯的精修磨可以避免表面缺陷的产生。Abstract: A research was carried out to investigate the as-cast,as-rolled and as-annealed metallographic structure as well as as-annealed mechanical property and surface defects of heat-resistant austenitic stainless steel coil 309S which was produced with smelting-rolling-annealing and pickling process.The results show that under the above three conditions,the steel is composed of austenite and high temperature residual ferrite that could not be eliminated by heat treatment.For the as-rolled and as-annealed structure,there is low content of ferrite near the surface and high content of ferrite in the core along the thickness direction.The product's mechanical properties are not affected by the high temperature residual ferrite.Fine grinding of the continuously cast slab can avoid surface defect of the product.
-
Key words:
- austenitic stainless steel /
- 309S /
- metallographic structure /
- mechanical property /
- surface defect
-

计量
- 文章访问数: 120
- HTML全文浏览量: 23
- PDF下载量: 2
- 被引次数: 0